Volume 30 Issue 2
Mar.  2013
Turn off MathJax
Article Contents

DIAO Hailin, BAI Linghai, TANG Xianming, MO Li, TANG Jixin, LUO Jianju. Pilot test drying process for Castanopsis hystrix lumber[J]. Journal of Zhejiang A&F University, 2013, 30(2): 240-244. doi: 10.11833/j.issn.2095-0756.2013.02.013
Citation: DIAO Hailin, BAI Linghai, TANG Xianming, MO Li, TANG Jixin, LUO Jianju. Pilot test drying process for Castanopsis hystrix lumber[J]. Journal of Zhejiang A&F University, 2013, 30(2): 240-244. doi: 10.11833/j.issn.2095-0756.2013.02.013

Pilot test drying process for Castanopsis hystrix lumber

doi: 10.11833/j.issn.2095-0756.2013.02.013
More Information
  • Corresponding author: DIAO Hailin
  • Received Date: 2012-03-13
  • Rev Recd Date: 2012-08-14
  • Publish Date: 2013-04-20
通讯作者: 陈斌, bchen63@163.com
  • 1. 

    沈阳化工大学材料科学与工程学院 沈阳 110142

  1. 本站搜索
  2. 百度学术搜索
  3. 万方数据库搜索
  4. CNKI搜索

Article views(3258) PDF downloads(1103) Cited by()

Related
Proportional views

Pilot test drying process for Castanopsis hystrix lumber

doi: 10.11833/j.issn.2095-0756.2013.02.013
    Corresponding author: DIAO Hailin

Abstract: To do Castanopsis hystrix wood drying pilot test,validation of pilot test drying schedule is correct,suitable for Castanopsis hystrix production and application of dry schedule. Forced air circulation for ordinary kiln drying,which is widely used in production,was utilized in a drying experiment of Castanopsis hystrix lumber with a given pilot drying schedule;Then,lumber dryness quality was evaluated according to the national standard (GB/T 6491-1999). Pilot test results showed that the average final moisture content of Castanopsis hystrix lumber was 7.24%;moisture content for deviation of thickness was 2.37%;the stress index was 4.12%;the average camber parallel to the grain of the wood was 0.17%;the camber perpendicular to the grain was 0.25%;twisting degree was 0.24%;the tile-shaped camber was 2.55%;the longitudinal crack degree was 3.31%;the section shrinkage rate was 5.793%;there was no internal cracking;the time of drying to a moisture content of 12% was 138 h (5.75 d);and drying speed was 0.31%h-1. Intermediate test drying benchmark was basic correct. Generally,the dryness quality of Castanopsis hystrix lumber was favorable and met the production requirements for wood products.[Ch,1 fig. 4 tab. 11 ref.]

DIAO Hailin, BAI Linghai, TANG Xianming, MO Li, TANG Jixin, LUO Jianju. Pilot test drying process for Castanopsis hystrix lumber[J]. Journal of Zhejiang A&F University, 2013, 30(2): 240-244. doi: 10.11833/j.issn.2095-0756.2013.02.013
Citation: DIAO Hailin, BAI Linghai, TANG Xianming, MO Li, TANG Jixin, LUO Jianju. Pilot test drying process for Castanopsis hystrix lumber[J]. Journal of Zhejiang A&F University, 2013, 30(2): 240-244. doi: 10.11833/j.issn.2095-0756.2013.02.013

Catalog

    /

    DownLoad:  Full-Size Img  PowerPoint
    Return
    Return